The systems are capable of operating in high-stress environments and feature encapsulation of materials with solid electrolyte coatings that can be designed to meet the increasingly demanding needs of any battery application. The solid electrolyte layer minimises the potential for the formation of an internal short circuit between electrodes to prevent ‘thermal runaway’, or the uncontrolled increase in battery cell temperature that can result in a fire or an explosion.
In addition, coating of the electrode materials reduces the stress on traditional polymer separators that are currently necessary components in commercial lithium-ion batteries and can allow for thinner separators designed for higher power devices. This advancement has the potential to reduce both the cost and weight of the battery device, while substantially increasing safety and lifetime.
Lab-scale testing of NREL’s hybrid solid-liquid electrolyte system has shown increased electrode durability and reliability without compromised electrochemical performance.
“This license agreement will allow Forge Nano to offer further customised lithium-ion battery materials for high performance devices by utilising our patented high-throughput ALD system that has already been successfully tested at the pilot scale and in large format pouch cells” said Paul Lichty, CEO of Forge Nano. “The incorporation of this technology into Forge Nano’s offering will lead to a substantial reduction in cost per unit energy of lithium-ion batteries.”
Ahmad Pesaran, whose team of engineers in NREL’s Energy Storage group invented the technology, added that the cells are less likely to fail, even in demanding, real-world conditions like high temperatures and fast recycle rates.
Forge Nano, formerly PneumatiCoat Technologies, is a Colorado-based company specialising in the scale-up and manufacturing of cost-effective Atomic Layer Deposition (ALD) encapsulated materials. Forge Nano presented its technology at the 2013 and 2017 NREL Industry Growth Forum, the nation’s premier clean energy investment event. A year later, NREL approached the company as a potential licensee after conducting a licensee search in the battery technology area.